In this article ,the drug-resistance of two kinds of medical rubber whose surfaces have been modified were investigated by ATR-FTIR and XPS. The experimental results show that the compositions of the two samples'surface and body are different. The surface is fluorinated rubber although the body is butyl rubber. The ratio of fluorine to carbon atom in sample Ii -1 is higher than that in sample I -1. The principal join between F and C is the form--CF2--in sample II -1,but in sample I -1 it is the form--CF2-- and--CHF--. The change for F/C of the different depth in sample II- 1 was relatively less than that in sample I -1 when they were etched by argon ion bundle in the same conditions.