Objective: This study evaluated color stability of acrylic denture teeth and base resins after 48 weeks of commercial denture cleanser simulation.
Materials and methods: Two brands of denture teeth (Trubyte Portrait IPN, TP; SR Vivodent DCL, SR) in shades A1, B1, and C1 and three acrylic base resins (Lucitone, LU; Paragon, PA; Valplast, VA) prepared to manufacturer's specifications were exposed 10 hours daily to four cleansers (Clorox Bleach, CB; Polident 3 minute, PO3; Efferdent, EF; and Kleenite, KL) and distilled water control, approximating consumer overnight use. Color measurements used the standard Commision International de l'Eclairage (International Commission on Illumination, CIE L*a*b*) color space (0, 4, 12, 24, 36, and 48 weeks.) Color differences (ΔE*) at 48 weeks were subjected to four-way analysis of variance (ANOVA). Mean values were compared with Fisher's (protected least significant difference) intervals (0.05 significance level).
Results: Mean color differences (ΔE*) demonstrated color changes in each material. ANOVA-indicated color changes in teeth were significantly affected by both cleansers and teeth brand (p < 0.05), but not shade. Color changes in base resins were significantly affected by cleansers (p < 0.05), but not brand alone. Overall, KL produced the least color change while CB and PO3 produced the most for all materials.
Conclusions: After 48 weeks of daily simulation, TP teeth were more color stable than SR in all cleansers except EF (p < 0.0001). Base resin VA was less color stable than LU and PA. Cleanser KL resulted in the lowest color changes.
Clinical significance: All tested materials yield clinically acceptable color changes (ΔE* < 3.5); all cleansing methods tested can be recommended, although Kleenite demonstrated the least change after 48 weeks.
© 2014 Wiley Periodicals, Inc.