To achieve highly efficient extraction of phosphorus (P) and comprehensive utilization of phosphate tailings, a two-stage leaching-precipitation method was proposed. Phosphate tailings primarily consisted of dolomite, fluorapatite, and quartz. During the first-stage leaching, the large majority of dolomite was selectively dissolved and the leaching efficiency of Mg reached 93.1 % at pH 2.0 and 60 °C. The subsequent second-stage leaching of fluorapatite was performed and the P leaching efficiency was 98.8 % at pH 1.5 and 20 °C, while the quartz remained in the residue. Through two-stage leaching, a stepwise leaching of dolomite and fluorapatite was achieved. After chemical precipitation, calcium phosphate with a high purity of 97.9 % was obtained; and the total recovery efficiency of P exceeded 98 %. The obtained calcium phosphate can be a raw material in the phosphorus chemical industry, while the Mg-rich leachate and the final quartz-rich residue have the potential for Mg extraction and the production of mortars or geopolymers, respectively. The two-stage leaching-precipitation process could significantly reduce the leaching costs, and enhance the reaction rates. It is expected to realize a volume reduction and efficient resource utilization of the phosphate tailings by using this sustainable and promising solution.
Keywords: P recovery; Phosphate tailings; Precipitation; Resource utilization; Two-stage leaching.
Copyright © 2024 Elsevier Inc. All rights reserved.