Li3PO4-Enriched SEI on Graphite Anode Boosts Li+ De-Solvation Enabling Fast-Charging and Low-Temperature Lithium-Ion Batteries.
Wang C, Xie Y, Huang Y, Zhou S, Xie H, Jin H, Ji H.
Wang C, et al.
Angew Chem Int Ed Engl. 2024 May 21;63(21):e202402301. doi: 10.1002/anie.202402301. Epub 2024 Apr 3.
Angew Chem Int Ed Engl. 2024.
PMID: 38482741
Li(+) de-solvation at solid-electrolyte interphase (SEI)-electrolyte interface stands as a pivotal step that imposes limitations on the fast-charging capability and low-temperature performance of lithium-ion batteries (LIBs). Unraveling the contributions of key constituent …
Li(+) de-solvation at solid-electrolyte interphase (SEI)-electrolyte interface stands as a pivotal step that imposes limitations on the fast …